This test method covers the determination of an asphalt binder’s resistance to ductile failure using a double-edge-notched tension test.
The test is conducted after thermal conditioning to determine the essential work of failure, the plastic work of failure, and an approximate critical crack tip opening displacement at a specified temperature and rate of loading.